Appearance |
Clear spherical beads |
Polymer Matrix Structure |
Styrene Crosslinked- DVB |
Type |
Macroporous Strongly Basic |
Functional Group |
R-N-(C4H9)3+Cl- |
Ionic Form |
Chloride |
Moisture Content (%) |
52-62 |
Capacity in Volume (mmol/ml) |
≥0.8 |
Capacity in Volume (mmol/g) |
≥3.0 |
Shipping Weight (g/ml) |
0.65-0.71 |
Density g/ml |
1.05-1.11 |
Screen size range | 0.315 – 1.25 mm ;50 – 16 mesh |
PH Range |
1 – 14 |
The High Temperature ℃ |
170 |
Total Capacity mmol/L |
≥ 1000 |
Backwash Rate |
50 to 75 percent Bed Expansion |
Regenerant Level |
2 to 15 lbs/ft3 |
Regenerant Concentration % |
2-10 |
Regenerant Flow Rate |
0.25 to 1.0 gpm/ft3 |
Regenerant Contact Time (min) |
30 minutes |
Fast Rinse Volume |
35 to 60 gal/ft3 |
Rinsing Flow Rate (m/h) | Same as regenerant flow rate |
Service Flow Rate | 2 to 4 gpm/ft3 |